Matsakaicin cikakken karɓar karɓar sifa a tarihi!
1. Bayyanar, girma da kuma dacewa da samfurin da aka ƙera
1. Ba a yarda da lahani a saman samfurin ba: ƙarancin abu, ƙonewa, saman fari, layin fari, haɗuwa, ƙyalli, fari (ko fasa, fasa), yin burodi, da wrinkles. .
2. Alamar Welding: Gabaɗaya, tsawon alamar walƙiya mai lanƙwasa bai wuce 5mm ba, kuma tsawon alamar walƙiya mai lankwasa ta musamman bai kai 15mm ba, kuma ƙarfin alamar walda na iya wuce gwajin amincin aiki. .
3. Karkacewa: Ba a yarda da tawaya a bayyane wuraren bayyanar ba, kuma an yarda da raguwa kadan a wuraren da ba a san su ba (ba jin diga ba) .
4. Kullum, flatness na kananan kayayyakin ne kasa da 0.3mm. Idan akwai abubuwan da ake buƙata na taro, dole ne a tabbatar da bukatun taron.
5. Kada ya kasance layukan iska ko furannin kayan abu a cikin bayyanannen bayyanar, kuma samfuran ya kamata gabaɗaya bashi da kumfa.
6. Yanayin yanayin yanayi da daidaiton girman samfurin ya kamata ya cika abubuwan da ake buƙata na zane mai inganci da inganci (ko fayil ɗin 3D). Samun haƙuri na samfur ya kamata ya dogara da tsarin haƙuri. Haƙurin girman shaft haƙuri ne mara kyau, kuma haƙurin girman rami tabbatacce haƙuri ne. Abokin ciniki yana da Kamar yadda ake buƙata, kamar yadda ake buƙata.
7. Kaurin bangon samfur: Gabaɗaya ana buƙatar kaurin bangon samfurin ya zama mai kaurin bango, matsakaicin bangon da ba matsakaici ba ya kamata ya cika buƙatun zane, kuma haƙurin ya zama -0.1mm bisa ga halaye na sifar.
8. Haɗin samfur: kwasfa na farfajiya da daidaitawar harsashi na ƙasa: daidaitaccen yanayin ƙasa bai kai 0.1mm ba, kuma kada a sami tarko. Ramuka, raƙuman ruwa da saman da suke da buƙatun daidaitawa dole ne su tabbatar da tsaka-tsakin dace da amfani da buƙatun.
Na biyu, bayyanar da sifar
1. Abubuwan da ke jikin sunan suna ya kammala, haruffan sun bayyana, kuma tsarin yana da kyau.
2. Yakamata a gyara sunan suna a ƙafa mai ƙira kusa da samfuri da kusurwar tunani. Rubutun sunan abin dogaro ne kuma ba sauki a cire ba.
3. Ya kamata a sanya bututun ruwa mai sanyaya bututun toshewa na roba, idan abokin ciniki ya buƙaci akasin haka, don Allah a bi abubuwan da ake buƙata. 4. Rufin ruwan sanyaya bai kamata ya fito daga farfajiyar tushe ba
5. Bututun ruwa mai sanyaya yana buƙatar sarrafa shi tare da takaddama. A counterbore diamita ne 25mm, 30mm da 35mm. Hanyar orifice tayi ado kuma yakamata ya zama iri daya. .
6. Ya kamata a sanya bakin ruwa mai sanyaya ruwa don shiga da fita.
7. Yiwa alama haruffa da lambobin Ingilishi girma fiye da 5/6, kuma matsayin ya zama 10mm kai tsaye ƙasa da famfo. Rubutun hannu ya zama a sarari, kyakkyawa, mai kyau, kuma ya daidaita tazara.
8. Kayan kwalliyar kayan kwalliya kada su shafar kwalliya da adana kayan kwalliya. Yayin shigarwa, akwai silinda masu fallasa, famfo, kayan sake saiti, da sauransu, waɗanda ya kamata a kiyaye su ta hanyar tallafar ƙafafu.
9. Dole ne a kafa kafa na goyan baya a kan ginshiƙin abin da yake jujjuyawar ƙafafun kafa, kuma za a iya ɗora dogayen ƙafafun ƙafa a kan ginshiƙan ɗin tare da ginshiƙan zaren waje na waje.
10. Girman ramin ejector na ƙirar ya kamata ya cika buƙatun na'urar da aka ƙayyade da allura. Ban da ƙananan ƙwayoyi, cibiyar ɗaya ba za a iya amfani da ita don fitarwa ba.
11. Yakamata zoben sanyawa ya zama abin dogaro. A diamita na zobe ne 100mm da 250mm. Zoben sanyawa ya fi 10-20mm girma sama da farantin ƙasa. Sai dai idan kwastomomi sun nema.
12. Matsakaicin waje na kayan kwalliyar yakamata ya cika bukatun injin da aka sanya masa allura.
13. Don kayan kwalliya tare da buƙatun fuskantarwa, ya kamata a yi amfani da kibiya don nuna alamar shigarwa akan samfurin farko ko samfurin baya. Ya kamata a sami "UP" kusa da kibiyar. Kibiyar da rubutu duk rawaya ne kuma tsayin font 50 mm.
14. Farfajiyar ginshiƙin ya kamata ba ta da rami, alamun tsatsa, zoben da ba su da yawa, tururin ruwa a ciki da waje, ramin mai, da sauransu, da lahani waɗanda ke shafar bayyanar.
15. Yakamata fasalin ya zama mai sauƙin hawa da jigilar kaya, kuma ba za'a rarraba sassan kayan ba yayin hawan, kuma kada zoben da ke ɗagawa ya tsoma baki tare da bututun ruwa, silinda na mai, sandar da aka sake saiti, da sauransu.
3. Kayan abu da taurin kai
1. moldaƙƙarfan sifa ya zama ginshiƙan tushe wanda ya dace da daidaito.
2. Mould forming parts and gating system (core, movable and gyara kayan masarufi abun saka, m abun sakawa, split cones, push rods, sprue hannayen riga) an yi su ne da kayan aiki tare da aiki sama da 40Cr.
3. Lokacin da ake yin robobi da suke lalata lahanin, ya kamata a sanya sassan da aka sassaka da kayan da ke jure wa lalata, ko kuma fuskar da ke yin yaren ya kamata ya ɗauki matakan anti-lalatawa.
4. Thearfin sassan da aka sassaka bai kamata ya zama ƙasa da 50HRC ba, ko kuma taurin ƙarfin jijiyar farfajiyar ya zama ya fi 600HV girma.
Hudu, fitar da, sake saitawa, cire fitar da murfin, cire
1. Fitar ya zama mai santsi, ba tare da matsi ba, kuma ba tare da sauti mara kyau ba.
2. Ya kamata saman saman da aka karkata ya goge, kuma saman da aka karkata ya kasa da ainihin farfajiyar.
3. Yakamata a samarda sassan zamiya da ramin mai, kuma farfajiyar tana bukatar nitrided, kuma taurin bayan bayan jiyya shine HV700 ko sama da haka.
4. Duk sandunan ejector yakamata su sami matsayin juyawa-juyawa, kuma kowane sandar ejector yakamata a kirga.
5. Nisan fitarwa ya kamata a iyakance ta hanyar toshiyar iyaka
6. Ya kamata a yi amfani da daidaitattun sassa don bazarar dawowa, kuma ƙarshen ƙarshen bazara bai kamata a goge ko yanke shi ba.
7. Zamewa da jawo-motsi ya kamata su sami iyakar bugun jini, ƙaramin silaid yana da iyaka ta bazara, idan bazara ba shi da sauƙi a girka, ana iya amfani da dunƙulen corrugated; Silinda-jan-dole yana da sauyawar bugun jini.
8. Gabaɗaya, ana amfani da ginshiƙan jagora don karkatar da siladin, kuma kusurwar gidan jagorar mai karkata ya zama ƙarami 2 ° ~ 3 ° fiye da kusurwar farfajiyar farfajiyar. Idan bugun darjewar ya yi tsayi da yawa, ya kamata a yi amfani da silinda mai don zane.
9. Lokacin da aka rufe ƙarshen ƙarshen ɓangaren da ke haifar da silinda, silinda ya kamata a sanye shi da injin kulle kansa.
10. Ya kamata a sami faranti masu jure lalacewa a ƙarƙashin manyan faifai masu faɗi fiye da mm 150. Kayan farantin da ba zai iya sawa ya zama T8A ba. Taurin bayan magani mai zafi shine HRC50-55. Faranti mai jure lalacewa ya fi 0.05-0.1 mm girma sama da babban fili. Buɗe tankin mai.
11. Kada sandar ejector ta motsa sama da kasa.
12. barara sandunan akan sandar sama, kuma alkiblar sandunan ya zama daidai, ta yadda sandunan suna da sauƙin cirewa daga samfurin.
13. Yankewa tsakanin ramin pin ejector da pin ejector, tsawon sashin sealing, da kuma yanayin yanayin rami na ejector ya zama daidai da bukatun ƙa'idodin kamfani masu dacewa.
14. Samfurin ya zama mai dacewa ga mai aiki don cire shi.
15. Lokacin da aka fitar da samfurin, yana da sauƙi a bi saman karkata, kuma ya kamata a dunƙule saman sandar ko kuma a ɗaura ta.
16. Babban toshe da aka gyara akan sandar sama ya zama tabbatacce kuma abin dogaro, ɓangaren da ba a kafa ba a kewayen da'irar ya kamata a sarrafa shi da gangaren 3 ° ~ 5 °, kuma ya kamata a gurɓata ƙananan sassan.
17. Kada a sami rarar baƙin ƙarfe a cikin ramin rarar mai a kan ginshiƙin juji.
18. facearshen fuskar komowar komo yana kwance kuma babu walda mai tabo. Babu kwantena a ƙasan kan amfrayo, walda tabo.
19. plateofar falon farantin farantin roba mai fa'ida daidai, kuma farantin ƙofar yana da sauƙi a buɗe.
20. Yakamata a tsara sandunan iyakoki masu ƙwananti uku a bangarorin biyu na shugabantar shigar da ƙirar, ko kuma a ɗora faranti a ginshiƙan don ƙirƙirar sandunan iyaka daga tsoma baki tare da mai aiki.
21. Yankin mai da wucewar iska ya zama santsi, kuma ya kamata a sake dawo da hidimar lantarki.
22. Ya kamata a buɗe tashar shaye shaƙ a ƙasan hannun riga.
23. Bai kamata a sami izinin sharewa ba.
5. Sanyaya da dumama tsarin
1, Tsarin sanyaya ko tsarin dumama yakamata ya kasance yana da cikakku.
2. Ya kamata hatimin ya zama abin dogaro, tsarin bai kamata ya zube ba a matsewar 0.5MPa, kuma yana da sauki a duba kuma a gyara.
3. Girman da siffar rami na hatimi da aka buɗe akan ginshiƙin yakamata ya cika buƙatun ƙa'idodin da suka dace.
4. Ya kamata a shafa man shafawa a zoben hatimi lokacin da aka sanya shi, kuma ya zama ya fi sama da saman ginshiƙin bayan an sanya shi.
5. Ya kamata a sanya masu raba tashan kwararar ruwa da mai ta kayan da ba sa saurin lalacewa.
6. Samfurin gaba da na baya yakamata suyi amfani da wadataccen ruwan sha.
Shida, tsarin zubowa
1, Saitin ƙofar bai kamata ya shafi bayyanar samfurin ba kuma ya haɗu da samfurin samfuran.
2. Ya kamata a tsara sashin masu tsere da tsayi yadda ya kamata, kuma ya kamata a taqaita aikin gwargwadon yadda zai yiwu a qarqashin tabbatar da ingancin samuwar, kuma ya kamata a rage yanki na giciye don taqaita lokacin cikawa da sanyaya lokaci. A lokaci guda, asarar filastik na tsarin zubowa ya zama mafi ƙarancin.
3. ofangaren mai gudu mai ɗaukar farantin farantin karfe uku a bayan bayan fage ya zama trapezoidal ko semicircular.
4. Maɓallin farantin karfe uku yana da abin fashewa akan faifan ƙofar, diamita na ƙofar ƙofar ya zama ƙasa da 3 mm, kuma kan ƙwallon yana da matakai mai zurfin 3 mm da aka sake shiga cikin farantin ƙofar.
5. Yakamata sandar jan ƙwallo ta ƙare a dogara, za a iya matse shi a ƙarƙashin zobe mai sanyawa, za a iya gyara shi da dunƙule mara kan kai, ko za a iya matsa shi da farantin matsi
6. atesofar ƙofa da masu gudu ya kamata a sarrafa su gwargwadon girman buƙatun zane, kuma ba a yarda da nika da injin goge ba.
7. gateofar ƙofa mai ma'ana ya kasance daidai da bukatun ƙayyadaddun bayanai.
8. Yakamata a sami kari a karshen karshen mai gudu a matsayin ramin sulke mai sanyi.
9. Zangarwar Z mai siffa kamar inverted sandar jan itace ya kamata ya sami miƙaƙƙiyar miƙaƙƙiya.
10. Ya kamata mai gudu a farfajiyar rabuwar ya zama zagaye, kuma ba za a iya daidaita misalan gaba da na baya ba.
11. Theofar latent a kan sandar ejector ba ta da ƙanƙancewar fuska.
12. A diamita da kuma zurfin da sanyi tutsar sulug for m kayayyakin kamata saduwa da zane nagartacce.
13. Maƙallan yana da sauƙin cirewa, babu alamar ƙofa akan bayyanar samfurin, kuma babu sauran ragowar a taron samfuran.
14. Don murfin ƙofar lankwasa mai lankwasa, ɓangarorin biyu na abin da aka saka ya kamata a nitrided, kuma taurin saman zai iya kaiwa HV700.
Bakwai, tsarin mai gudu mai zafi
1. Tsarin wayoyi na mai gudu mai zafi ya zama mai dacewa don sauƙin kulawa, kuma lambar wayoyi ya zama wasiƙa ɗaya-da-ɗaya.
2. Ya kamata a gwada mai gudu mai zafi don kare lafiya, kuma juriya mai rufin ƙasa ya zama ya fi 2MW girma.
3. daidaitattun sassa ya kamata a karɓa don zafin jiki kula majalisar, zafi bututun ƙarfe da zafi mai gudu.
4. Babban haɗin tashar jirgin ruwa mai gudana an haɗa shi tare da mai gudu mai zafi tare da zaren, kuma saman ƙasa yana cikin haɗuwa da mai gudu mai zafi don hatimi.
5. Mai tsere mai zafi yana cikin kyakkyawar mu'amala da farantin dumama ko sandar dumama, kuma an tsaftace farantin dumama da dunƙule ko sanduna, kuma saman ya yi daidai.
6. Ya kamata a yi amfani da thermocouple mai nau'in J kuma ya dace da mitar kula da yanayin zafin jiki.
7. Kowane rukuni na abubuwan dumama yakamata a sarrafa su ta thermocouples, kuma yakamata a daidaita matsayin thermocouples ɗin yadda ya kamata.
8. Bututun ƙarfe ya kamata ya cika buƙatun ƙira.
9. Ya kamata mai gudu mai zafi ya kasance an dogara da shi, aƙalla fil biyu na sanyawa, ko kuma an daidaita shi da sukurori.
10. Ya kamata a sami pad na rufi tsakanin mai gudu mai zafi da kuma samfurin.
11. Kuskure tsakanin saitin zafin jiki na mitar sarrafa zafin jiki da ainihin zazzabin nuni ya zama ƙasa da ± 5 ° C, kuma ikon zafin ya zama mai da hankali.
12. Ramin shigar da rami da bututun ƙarfe ya kamata ya ratsa.
13. Waya mai zafi mai zafi ya kamata a haɗa shi kuma a rufe shi da farantin matsi.
14. Akwai kwasfansu guda biyu masu irin wannan bayanin, wanda yakamata ayi masu alama a fili.
15. Layin sarrafawa ya zama mai sheathed ba lalacewa ba.
16. Tsarin tsarin kula da zafin jiki abin dogaro ne, kuma sukurorin ba sako-sako suke ba.
17. An shigar da soket a kan bakelite kuma ba zai iya wuce matsakaicin girman samfurin ba.
18. Wayoyin dole ne ba za a fallasa su a waje.
19. Duk wuraren da mai gudu mai zafi ko samfuri yake cikin ma'amala da wayoyi yakamata sun sami sauye-sauye zagaye.
20. Kafin a tattara samfuri, babu wata da'irar buɗewa ko gajeren hanya a cikin dukkanin da'irai.
21. Duk wayoyi ya kamata a haɗa su daidai, tare da kyakkyawan aikin rufi.
22. Bayan an shigar da samfuri kuma an liƙe shi, ya kamata a sake bincika dukkan da'ira tare da multimeter.
8. Sashin bangare, farfajiyar rabuwar kai, sharar tsagi
1. Kada a sami rashin daidaito, ramuka, tsatsa da sauran lahani da suka shafi bayyanar a farfajiyar gaban da na baya.
2. Abun da aka saka ya dace da firam mai siffar, kuma yakamata a sami yarda kasa da 1 mm a kewayen sasanninta.
3. Farkon rabuwar ya kasance mai tsafta. Babu keken motsawa mai motsi don kauce wa ramuka, kuma ɓangaren hatimin ba shi da ɗigo.
4. Zurfin dusar sharar ya zama ƙasa da ƙimar ambaliyar filastik.
5. Bincike da rarraba abubuwan da ake sakawa ya kamata su kasance a wuri, tare da sanya mai sassauci da amintaccen matsayi.
6. Abubuwan da ake sakawa, abubuwan da ake sakawa, da sauransu yakamata a sanya su cikin abin dogaro kuma a gyara su, ya kamata a hana gabobin zagaye su juyawa, kuma kada a sanya zanen tagulla ko ƙarfe a ƙarƙashin abubuwan da ake sakawa.
7. endarshen fuskar sandar ejector daidai yake da ainihin.
8. Bangaren da yake samarwa na gaba da na baya ba shi da wata nakasa kamar ta karkashin kasa da kuma kayan kwalliya.
9. Ya kamata a tura haƙarƙarin haƙarƙarin cikin sauƙi.
10. Don kayayyakin keɓaɓɓen rami, sassan hagu da dama suna da daidaito, kuma yakamata a nuna L ko R. Idan abokin ciniki yana da buƙatu don matsayi da girma, ya kamata ya cika buƙatun abokin ciniki. Gabaɗaya, ƙara shi a inda baya shafar bayyanar da taron. Girman rubutu shine 1/8.
11. Farfajiyar murdadden ginshiƙin yakamata ta kasance, kuma ya kamata a taɓa fiye da 75% na yankin.
12. Ya kamata a shirya sandunan ejector kusa da bangon gefe da gefan hakarkarin da shuwagabannin, sannan a yi amfani da sandunan ejector manya.
13. Don sassa ɗaya, lambobi 1, 2, 3, da sauransu, ya kamata a nuna su.
14. Kowane farfajiyar tuntube, farfajiyar shiga, da kuma bangaren rabuwar ya kamata ayi bincike a kuma daidaita su a wurin.
15. Banbancin farfajiyar farfajiyar farfajiyar ya kamata ya cika ka'idodin zane. 10-20mm don matsakaitan matsakaici, 30-50 mm don manyan ƙira, kuma sauran sassan an kera su don kauce wa sarari fanko.
16. Tsarin fata da sandblasting ya kamata ya cika bukatun abokin ciniki daidai.
17. Don samfuran da ke da buƙatu don bayyana, sukurorin da ke kan samfuran ya kamata su sami matakan kariya.
18. Ya kamata a yi amfani da bututun Jack don ginshiƙan ginshiƙai tare da zurfin fiye da 20 mm.
19. Girman bangon samfurin ya zama iri ɗaya, kuma ya kamata a sarrafa karkatarwa ƙasa da ± 0.15 mm.
20. Faɗin haƙarƙarin ya kamata ya zama ƙasa da kashi 60% na kaurin bangon fuskar waje
21. Abubuwan da aka saka a saman rufin da silar da darjewa ya kamata su sami hanyar gyarawa abin dogaro.
22. An sanya abin da ke gaban gaba a cikin na baya ko kuma na baya an saka shi a cikin na gaban, kuma ya kamata a kulle bangarorin tare da jirage masu karkata da kuma kera injina don kaucewa iska.
Nine, allurar gyare-gyaren allura
1, The mold kamata da kwanciyar hankali na allura gyare-gyaren samarwa da kuma repeatability na aiwatar siga daidaitawa a cikin kewayon al'ada allura gyare-gyaren tsari yanayi.
2. Matsayin allura yayin samar da allurar ƙira ya kamata ya zama ƙasa da kashi 85% na injin allurar ƙira mai ƙira matsakaicin matsin lamba.
3. Gudun saurin allurar samar da allura mai saurin canzawa, saurin allura na bugun kwata uku ba kasa da 10% na girman saurin allura da aka yiwa sihiri ko fiye da 90% na yawan saurin allura da aka yiwa alama.
4. Matsayin riƙewa na ƙirar a yayin gyaran allurar ya kamata ya zama ƙasa da 85% na ainihin matsakaicin matsin lamba.
5. lamarfin ƙwanƙolin ƙira a yayin samar da gyarar allura ya zama ƙasa da kashi 90% na ƙarfin clamping na samfurin da ake buƙata.
6. Yayin aikin samar da allura, allurar da bututun ƙarfe ya kamata a fitar cikin sauƙi kuma cikin aminci (lokaci bai wuce dakika 2 kowannensu ba).
7. Don kayan kwalliya tare da abun sakawa, abubuwan sakawa suna da sauƙin shigarwa kuma an gyara abubuwan da ake sakawa cikin aminci yayin samarwa.
10. Marufi da safara
1 Yakamata a tsabtace ramin da aka tsara tare da fesa shi da mai na anti-tsatsa.
2. Yakamata a saka sassan zamiya.
3. Ya kamata a rufe mashigar ruwa ta sprue da man shafawa.
4. Ya kamata a tsara kayan kwalliyar tare da matattarar abubuwa, kuma bayanai dalla-dalla sun dace da ƙirar ƙira.
5. Spaangarorin kayayyakin gyara da kayan sawa yakamata su cika, tare da cikakken jerin sunayen masu kaya
6. Ya kamata a dauki matakan rufewa don hana bakin abu daga shiga ruwan mulmula, ruwa, gas, da mashigar lantarki da mashigai;
7. Fesa fenti a farfajiyar farfajiyar, kamar yadda mai bukata ya bukata.
8. Samfura yakamata a sanya su cikin kwalliyar hana ruwa, ruwa mara kwari, da kwalliya mai kariya, kamar yadda kwastomomi ke bukata.
9. Zanen samfurin zane, zane-zane na tsari, sanyaya da zane tsarin zafin jiki, zane mai gudu mai zafi, sassan kayan masarufi da kayan kwalliyar kayan kwalliya, umarnin aiki, rahotannin gwajin kwalliya, takaddun duba ma'aikata, da takardun lantarki duk yakamata su cika.
Da fatan za a adana tushe da adireshin wannan labarin don sake bugawa: Matsakaicin cikakken karɓar karɓar sifa a tarihi!
Minghe Kamfanin 'Yan Wasa Masu Mutu aka sadaukar domin tsirar da samar da inganci da kuma high yi Gyare sassa (karfe mutu simintin sassa Range yafi hada da Thin-Wall Mutu Wasa,Hot Chamber Mutu Wasa,Cold Chamber Mutu Wasa), Zagaye Sabis (Mutuwar 'Yan Wasa,CNC machining,Motsa Motsa, Jiyya na sama) .Adadin al'ada Aluminium ya mutu, magnesium ko Zamak / zinc mutu simintin gyare-gyare da sauran buƙatun simintin maraba don tuntube mu.
Karkashin kulawar ISO9001 da TS 16949, Ana aiwatar da dukkan matakai ta hanyar daruruwan injunan jefa simintin da suka mutu, injunan axis 5, da sauran kayan aiki, tun daga masu fashewa zuwa na’urar Ultra Sonic masu wanki.Minghe ba kawai tana da kayan aiki na zamani ba amma kuma tana da kwararru ƙungiyar ƙwararrun injiniyoyi, masu aiki da sufetoci don tabbatar da ƙirar abokin ciniki ta zama gaskiya.
Manufactureran kwangilar masana'antar mutu. Abubuwan haɓakawa sun haɗa da sassan sanyi na sassan mutuɗar aluminum daga 0.15 lbs. zuwa 6 lbs., saurin canje-canje da aka saita, da aikin inji. Sabis-ƙarin ayyuka sun haɗa da gogewa, faɗakarwa, lalatawa, fashewar harbi, zane, zane, rufi, haɗuwa, da kayan aiki. Abubuwan da aka yi aiki tare sun haɗa da allo irin su 360, 380, 383, da 413.
Zinc ya mutu don jefa ƙirar ƙira / sabis na injiniya tare. Custom manufacturer na daidaici tutiya mutu simintin gyaran kafa. Castananan 'yan simintin gyare-gyare, pressurean ƙwanƙwasa masu juzu'in juzu'in simintin gyare-gyaren juzu'ai, ƙera simintin gyare-gyare na al'ada, ɓangaren mutu da' yan wasa masu mutuwa masu zaman kansu da ƙofar da aka hatimce za a iya ƙera su. Za'a iya kerarrar 'yan simintin a tsayi da faɗi har zuwa 24 a ciki. A cikin +/- 0.0005 a cikin. Haƙuri.
ISO 9001: 2015 bokan masana'anta ta mutu magnesium, Abubuwan haɓaka sun haɗa da matsin lamba na magnesium mai matsi mai yawa har zuwa tan 200 mai ɗumi mai zafi & 3000 ton mai sanyi, ƙirar kayan aiki, gogewa, gyare-gyaren, inji, foda & zanen ruwa, cikakken QA tare da damar CMM , taro, marufi & isarwa.
ITAF16949 bokan. Servicearin Sabis ɗin Gyare Hadawa zuba jari,yashi,Kushin nauyi, Stauren ɓoye ɓoye,Siffar Centrifugal,Cast Vacuum,Dindindin Mould Gyare, .Hanyoyin iyawa sun hada da EDI, taimakon injiniya, ingantaccen samfuri da aiki na sakandare.
Fitar Masana'antu Abubuwan Nazarin sassa don: Motoci, Bikes, Jirgin sama, kayan kiɗa, Jirgin ruwa, Na'urorin hangen nesa, na'urori masu auna sigina, na'urori masu auna sigina, Na'urori, Kayan lantarki, ,unshi, Clocks, Inji, Injiniya, Kayan Kaya, Kayan Jiki, Jigs, Telecom, Haske, Kayan aikin likita, Na'urar daukar hoto, Robobi, Sassaka, kayan sauti, kayan wasanni, Kayan aiki, Kayan wasa da ƙari.
Me Zamu taimake ku yi gaba?
Je zuwa Shafin Farko Don Mutu Wasa China
→Sassan Kasuwanci-Gano abin da muka aikata.
→ Tallan kwankwasiyya Game da Ayyukan Gyare Mutuwa