Mutu simintin mutu nasa ne da wani irin simintin ruwa mutu ƙirƙira da musamman mutu simintin mutu ƙirƙira na'ura. Domin mutu Fitar, mutu simintin kayan, mutu simintin inji da mutu ba makawa. Don haɓaka ingantaccen samarwa, ingancin iri da fa'idodin tattalin arziƙi, da kuma tsawaita rayuwar sabis na mutu mutu, amfani da kiyaye mutuƙar mutu yana da mahimmanci.
Daidai amfani da kiyaye mutu simintin mutu
1. Ya kamata a rage saurin sanyaya da dumama injin ɗin gwargwadon iko, kuma a ci gaba da samarwa gwargwadon iko. An haramta allurar saurin sauri a cikin yanayin sanyi mai sanyi.
A cikin aiwatar da mutu-simintin, mutu-simintin mutu ya kasance cikin yanayin gajiya mai raɗaɗi na faɗaɗa zafi da raguwar sanyi, kuma yanayin zafin ramin yana canzawa daga 160 ℃ zuwa 350 ℃. Mutuwar tana saurin sanyaya da zafi, kuma ba a daina faɗaɗa zafi da ƙanƙancewa, yana haifar da lalacewar gajiya na mutu. Koyaya, lokacin da aka fara samarwa a cikin yanayin sanyi mai sanyi, zafin zafin yana fara tashi daga ƙarancin zafin jiki, bambancin zafin yana ƙaruwa, haɓaka ƙirar da ƙanƙancewa yana ƙaruwa, kuma gajiya mai ƙyalƙyali yana ƙaruwa daidai, wanda zai hanzarta lalacewar ƙirar da gajarta. rayuwar mold. Don haka, yakamata a ci gaba da samarwa gwargwadon iko a cikin samar da simintin gyare-gyare don rage saurin sanyaya da dumama mutuƙar gwargwadon iko, don tsawaita rayuwar mutu'a.
Bugu da ƙari, a cikin yanayin sanyi mai sanyi, ƙirar ba ta isa yawan zafin da ake samarwa, kuma rata tsakanin sassan ƙirar tana da girma. A wannan yanayin, an haramta shi sosai don buɗe allurar sauri da matsin lamba. In ba haka ba, sassan rarrabuwar kawunan mutuƙar, gami da toshewar faifai, ramin fil ɗin ejector da sauransu, suna da sauƙin shigar da takardar aluminium, don haka yana lalata ƙirar kuma yana shafar rayuwar mutu'a.
2. Yi ƙoƙarin rage saurin allura, takamaiman matsin lamba da tasirin mutuwa.
A cikin samar da simintin mutu, saurin allura ba kawai yana shafar saurin cikawa da saurin ƙofar ba, har ma yana ƙara ƙimar tasirin tasiri lokacin da saurin allura ya yi yawa. Sabili da haka, saurin allura yana da girma, saurin ƙofar allura yana da sauri, za a ƙara ƙaruwa da ƙirar, ƙimar ƙimar tasiri za ta ƙaru, ƙarfin tasirin ƙirar zai ƙaru, kuma rayuwar ƙirar za ta ragu sosai. . Don haka, lokacin da muka daidaita tsarin mutuƙar simintin, yakamata mu rage saurin allurar gwargwadon iko a ƙarƙashin yanayin tabbatar da ingancin samfurin, wanda yana da matukar mahimmanci don inganta rayuwar mutu da fa'idar tattalin arziƙin kamfanonin mutuƙar simintin. A halin yanzu, injin ɗin da ya mutu yana sanye da injin birki na allura, wanda yana da fa'ida sosai don rage ƙimar tasirin tasiri, rage ƙarfin tasirin da injin ke haifarwa, da inganta rayuwar mutu'a.
Matsakaicin matsin lamba shima muhimmin sigogi ne a cikin tsarin simintin mutu'a. Dangane da buƙatun inganci da halayen simintin gyare-gyare, takamaiman matsin lamba yana cikin kewayon 400-900 kg / cm2. Lokacin da zazzabi ya wuce 900 kg / cm2, yana da ɗan tasiri akan ingancin simintin ciki. Koyaya, idan matsi na allura ya yi yawa, ba kawai zai haɓaka ƙarfin haɓaka ƙirar ba, amma kuma zai sa ƙarfin faɗaɗa ya wuce ƙarfin kulle kayan aikin injin, wanda ke haifar da tashar tashar aluminum. A lokaci guda kuma, idan mutuƙar tana ɗauke da babban ƙarfi, hakanan zai lalata ƙirar ko ta rage rayuwar ƙirar. Sabili da haka, a cikin ƙere-ƙere, ya kamata mu mai da hankali sosai ga ƙimar allura fiye da yadda allurar take. Kamar yadda adadin allura ba shi da sauƙi a lura, galibi ana yin watsi da shi. A zahiri, takamaiman matsin lamba allura ce mai mahimmanci a cikin tsarin simintin mutuwa, wanda ba wai kawai yana shafar ingancin simintin ba, har ma yana da babban tasiri akan rayuwar mutu'a. Wannan batu ya kamata a fi mai da hankali da shi ta hanyar masana'antar simintin mutuwa.
3. Yayin aiwatar da amfani da injin, yakamata a tsabtace fatar blister da aluminium a cikin lokaci don hana ƙyallen ya lalace.
A cikin amfani da ƙirar, ƙyallen galibi yana bayyana nade -nade da fatar aluminium saboda dalilai daban -daban. A wannan lokacin, dole ne a tsabtace shi cikin lokaci, in ba haka ba ƙirar za ta lalace idan an ci gaba da samarwa. Musamman a cikin shinge mai zamewa, idan nunin faifai ya shiga cikin takardar aluminium, toshewar zamewar za ta rushe kuma ta lalace saboda babban ƙarfin matattarar injin simintin mutu. Don haka, idan aka sami irin waɗannan matsalolin, ya zama dole a tsabtace injin a cikin lokaci, gano abubuwan da ke haddasawa da gyara ƙirar a cikin lokaci. In ba haka ba, rayuwar sabis na mutu zai yi tasiri sosai idan mutuwar ta lalace.
4. Ya kamata a rage zafin zafin da ke narkar da aluminium gwargwadon iko don inganta rayuwar sabis na mutu.
Zazzabi mai ɗorewa na aluminium mai ruwa a cikin simintin mutuƙar ba kawai yana shafar ingancin simintin ba, har ma yana shafar rayuwar sabis na mutu simintin mutu. Gabaɗaya, zazzabi mai zuƙowa na aluminum aluminum shine digiri 630-720. Don sassa daban -daban, yakamata mu zaɓi ƙananan zazzabi mai ɗorewa gwargwadon abin da zai yiwu, wanda ba kawai zai iya adana kuzari ba, har ma ya tsawaita rayuwar sabis na mutu mutu. Saboda mafi girman zafin jiki na aluminium mai ruwa, mafi girman ɓarna na ƙirar, mafi girman kewayon filin zazzabi yana canzawa, mafi girman faɗaɗawar zafi da ƙuntatawa, mafi girman gajiya na ƙirar, mafi sauƙin lalacewa. Saboda haka, yana da fa'ida don tsawaita rayuwar sabis na mutu simintin mutu ta yadda yakamata rage zafin zazzabin aluminium.
5. Ƙarfafa kulawar ƙirar, kiyayewa na yau da kullun, tempering na yau da kullun na ƙwanƙwasa rami.
Mutuwar simintin mutu ya kasance cikin matsanancin matsin lamba, babban gudu, babban zafin ci gaba mai ɗorewa, yanayin amfani ba shi da kyau. Lokacin aiwatar da amfani, ƙirar za ta haifar da lalacewa ko ɓoyayyen matsala. Sabili da haka, yana da matukar mahimmanci a ƙarfafa kulawar ƙirar, a kula da ƙirar a kai a kai, maye gurbin sassan da suka lalace, maye gurbin ɓangarorin masu rauni, tsaftace hanyar zamewa, ramin pin ejector, da sauransu yana da matukar mahimmanci don tabbatar da amincin amincin mold a cikin mutu-simintin samarwa, kuma yana iya tsawaita rayuwar sabis na mold.
A lokaci guda, saboda mutuƙar simintin yana shafar kullun, yana ƙaruwa da raguwa, za a samar da sabon damuwa na ciki. Idan ba a kawar da shi cikin lokaci ba, murfin mutuƙar yana da sauƙin fashewa ko fashewa. Don haka, ita ma hanya ce mai mahimmanci don tsawaita rayuwar mutu'a ta hanyar rage damuwa a kai a kai. Gabaɗaya, zafin zafin farko yakamata a aiwatar dashi bayan lokutan ƙirar 3000-5000 bayan an yi amfani da injin. A nan gaba, gwargwadon amfani da halin da ake ciki, gabaɗaya kowane ƙirar ƙira na 10000, ramin ƙyallen don aiwatar da matsanancin damuwa, wanda zai iya ƙara tsawon rayuwar sabis na ƙirar.
Da fatan za a adana tushe da adireshin wannan labarin don sake bugawa:Hanyar Kulawa da Mutuwar Molding Mould
Minghe Kamfanin 'Yan Wasa Masu Mutu aka sadaukar domin tsirar da samar da inganci da kuma high yi Gyare sassa (karfe mutu simintin sassa Range yafi hada da Thin-Wall Mutu Wasa,Hot Chamber Mutu Wasa,Cold Chamber Mutu Wasa), Zagaye Sabis (Mutuwar 'Yan Wasa,CNC machining,Motsa Motsa, Jiyya na sama) .Adadin al'ada Aluminium ya mutu, magnesium ko Zamak / zinc mutu simintin gyare-gyare da sauran buƙatun simintin maraba don tuntube mu.
Karkashin kulawar ISO9001 da TS 16949, Ana aiwatar da dukkan matakai ta hanyar daruruwan injunan jefa simintin da suka mutu, injunan axis 5, da sauran kayan aiki, tun daga masu fashewa zuwa na’urar Ultra Sonic masu wanki.Minghe ba kawai tana da kayan aiki na zamani ba amma kuma tana da kwararru ƙungiyar ƙwararrun injiniyoyi, masu aiki da sufetoci don tabbatar da ƙirar abokin ciniki ta zama gaskiya.
Manufactureran kwangilar masana'antar mutu. Abubuwan haɓakawa sun haɗa da sassan sanyi na sassan mutuɗar aluminum daga 0.15 lbs. zuwa 6 lbs., saurin canje-canje da aka saita, da aikin inji. Sabis-ƙarin ayyuka sun haɗa da gogewa, faɗakarwa, lalatawa, fashewar harbi, zane, zane, rufi, haɗuwa, da kayan aiki. Abubuwan da aka yi aiki tare sun haɗa da allo irin su 360, 380, 383, da 413.
Zinc ya mutu don jefa ƙirar ƙira / sabis na injiniya tare. Custom manufacturer na daidaici tutiya mutu simintin gyaran kafa. Castananan 'yan simintin gyare-gyare, pressurean ƙwanƙwasa masu juzu'in juzu'in simintin gyare-gyaren juzu'ai, ƙera simintin gyare-gyare na al'ada, ɓangaren mutu da' yan wasa masu mutuwa masu zaman kansu da ƙofar da aka hatimce za a iya ƙera su. Za'a iya kerarrar 'yan simintin a tsayi da faɗi har zuwa 24 a ciki. A cikin +/- 0.0005 a cikin. Haƙuri.
ISO 9001: 2015 bokan masana'anta ta mutu magnesium, Abubuwan haɓaka sun haɗa da matsin lamba na magnesium mai matsi mai yawa har zuwa tan 200 mai ɗumi mai zafi & 3000 ton mai sanyi, ƙirar kayan aiki, gogewa, gyare-gyaren, inji, foda & zanen ruwa, cikakken QA tare da damar CMM , taro, marufi & isarwa.
ITAF16949 bokan. Servicearin Sabis ɗin Gyare Hadawa zuba jari,yashi,Kushin nauyi, Stauren ɓoye ɓoye,Siffar Centrifugal,Cast Vacuum,Dindindin Mould Gyare, .Hanyoyin iyawa sun hada da EDI, taimakon injiniya, ingantaccen samfuri da aiki na sakandare.
Fitar Masana'antu Abubuwan Nazarin sassa don: Motoci, Bikes, Jirgin sama, kayan kiɗa, Jirgin ruwa, Na'urorin hangen nesa, na'urori masu auna sigina, na'urori masu auna sigina, Na'urori, Kayan lantarki, ,unshi, Clocks, Inji, Injiniya, Kayan Kaya, Kayan Jiki, Jigs, Telecom, Haske, Kayan aikin likita, Na'urar daukar hoto, Robobi, Sassaka, kayan sauti, kayan wasanni, Kayan aiki, Kayan wasa da ƙari.
Me Zamu taimake ku yi gaba?
Je zuwa Shafin Farko Don Mutu Wasa China
→Sassan Kasuwanci-Gano abin da muka aikata.
→ Tallan kwankwasiyya Game da Ayyukan Gyare Mutuwa
By Minghe Mutu Wasa Wasa | Categories: Labarai masu Taimakawa |Material Tags: Gyare Aluminum, Zinc Gyare, Fitar Magnesium, Castan Wasanni, Bakin Karfe Cast, Fitar tagulla,Gyare Tagulla,Fitar Bidiyo,Tarihin Kamfanin,Aluminum Mutu Gyare | Comments Off