Takaita abubuwan canzawa da hanyoyin sarrafa nau'in wutar makera
Nau'in sarrafa wutar makera na yau da kullun yana nuna yanayin bangon ciki mai santsi da fata mai kauri. Koyaya, a cikin samar da wutar makera na gaske, saboda tasirin canje -canje a cikin tsarin slagging, tsarin caji, tsarin samar da iska, tsarin zafi, da albarkatun ƙasa na waje, ƙirar wutar makera mai aiki da wuta za ta sami canje -canje kamar tsayawa ko ƙyalli. wanda zai shafi wutar makera. Wannan zai haifar da ɓarkewar ɓarna mai ɓarna, wanda kuma zai haifar da lalacewar babban yanki a kan matattarar sanyaya.
Babban dalilan adhesion bangon makera sune:
1. Kayan albarkatun ƙasa ya ƙunshi babban foda, iskar gas ba ta haɓaka, kuma bututun gefen yana faruwa;
2. Tsarin slagging ba shi da tsayayye, aikin slag yana canzawa sosai, kuma raunin ƙarfe-ƙarfe mara kyau ne, wanda yake da sauƙi ya sa bangon tanderun ya makale;
3. Kula da zafin zafin wutar makera, manyan juye -juye, da sauye -sauye na wutar makera mai narkewa.
4. Ƙarfafa dogon ƙarfe na baƙin ƙarfe na baƙin ƙarfe da ƙaramin ƙarfe yana da girma, kuma raunin slag mara kyau ne;
5. Ruwan bangon sanyaya ko canje -canje a sanyaya matsin ruwa da zafin ruwa yana haifar da tsananin sanyaya;
6. Tsarin zane ba shi da ma'ana, yana haifar da iska ta cikin gida ko bututun bututu.
Babban abubuwan da ke haifar da fatar fatar bangon makera ya fado a cikin babban yanki shine: tsarin samar da iska da tsarin caji ba su da ma'ana, kuma iskar iska tana tasowa; canjin tsarin sanyaya yana haifar da ƙarancin sanyaya ƙasa, kuma ba za a iya kafa fatar slag ba.
Lokacin da yanayin makera ya canza, dole ne a ɗauki matakan cikin lokaci. Hanyoyin sarrafawa gaba ɗaya da aka karɓa sune:
1. Halayen rarraba suna ƙayyade rarrabawar iskar gas, wanda hakan ke ƙayyade rarraba filin zafin jiki a cikin tanderu da siffa da matsayi na yankin reflow. Musamman halayen reflow na cajin a bangon makera zai sa fatar fata ta yi kauri ko ta faɗi. Daidaita tsarin rarrabawa da ingantaccen sarrafawa na rarraba iskar gas sune mahimman hanyoyi don dawo da nau'in murhun wutar kamar yadda aka saba.
Lokacin da bangon makera ya makale, yakamata a ɗauki manyan matakan don sanya gefen, kuma yakamata a haɓaka iskar gefen. Lokacin da fatar fatar ta fado daga bangon makera, yakamata a ɗauki matakan matsin lamba don sarrafa iskar gas.
2. Sarrafa zafin wutar makera da maƙarƙashiya, bi da mannewar bangon makera, yadda yakamata sarrafa zafin wutar makera a matakin ƙima mafi girma, tsananin hana ƙarancin zafin zafin wutar makera, rage mahimmancin slag, da abun cikin sulfur na baƙin ƙarfe alade galibi aji na biyu ƙarfe don tabbatar da kyau Ruwa na baƙin ƙarfe.
3. Sarrafa tsananin sanyaya. Lokacin da fatar slag ba ta da sauƙi ta zama lokacin da fatar fatar ta faɗi, yakamata a ƙara matsin ruwan don ƙara ƙarfin sanyaya sashi. Lokacin da haɗin gwiwa ya faru, yakamata a rage matsin ruwan yadda yakamata don rage ƙarfin sanyaya ɓangaren.
4. A lokacin da ake mu'amala da manne na ɓangaren ƙasa, a wanke tanderu da kyau
Da fatan za a adana tushe da adireshin wannan labarin don sake bugawa:Takaita abubuwan canzawa da hanyoyin sarrafa nau'in wutar makera
Minghe Kamfanin 'Yan Wasa Masu Mutu aka sadaukar domin tsirar da samar da inganci da kuma high yi Gyare sassa (karfe mutu simintin sassa Range yafi hada da Thin-Wall Mutu Wasa,Hot Chamber Mutu Wasa,Cold Chamber Mutu Wasa), Zagaye Sabis (Mutuwar 'Yan Wasa,CNC machining,Motsa Motsa, Jiyya na sama) .Adadin al'ada Aluminium ya mutu, magnesium ko Zamak / zinc mutu simintin gyare-gyare da sauran buƙatun simintin maraba don tuntube mu.
Karkashin kulawar ISO9001 da TS 16949, Ana aiwatar da dukkan matakai ta hanyar daruruwan injunan jefa simintin da suka mutu, injunan axis 5, da sauran kayan aiki, tun daga masu fashewa zuwa na’urar Ultra Sonic masu wanki.Minghe ba kawai tana da kayan aiki na zamani ba amma kuma tana da kwararru ƙungiyar ƙwararrun injiniyoyi, masu aiki da sufetoci don tabbatar da ƙirar abokin ciniki ta zama gaskiya.
Manufactureran kwangilar masana'antar mutu. Abubuwan haɓakawa sun haɗa da sassan sanyi na sassan mutuɗar aluminum daga 0.15 lbs. zuwa 6 lbs., saurin canje-canje da aka saita, da aikin inji. Sabis-ƙarin ayyuka sun haɗa da gogewa, faɗakarwa, lalatawa, fashewar harbi, zane, zane, rufi, haɗuwa, da kayan aiki. Abubuwan da aka yi aiki tare sun haɗa da allo irin su 360, 380, 383, da 413.
Zinc ya mutu don jefa ƙirar ƙira / sabis na injiniya tare. Custom manufacturer na daidaici tutiya mutu simintin gyaran kafa. Castananan 'yan simintin gyare-gyare, pressurean ƙwanƙwasa masu juzu'in juzu'in simintin gyare-gyaren juzu'ai, ƙera simintin gyare-gyare na al'ada, ɓangaren mutu da' yan wasa masu mutuwa masu zaman kansu da ƙofar da aka hatimce za a iya ƙera su. Za'a iya kerarrar 'yan simintin a tsayi da faɗi har zuwa 24 a ciki. A cikin +/- 0.0005 a cikin. Haƙuri.
ISO 9001: 2015 bokan masana'anta ta mutu magnesium, Abubuwan haɓaka sun haɗa da matsin lamba na magnesium mai matsi mai yawa har zuwa tan 200 mai ɗumi mai zafi & 3000 ton mai sanyi, ƙirar kayan aiki, gogewa, gyare-gyaren, inji, foda & zanen ruwa, cikakken QA tare da damar CMM , taro, marufi & isarwa.
ITAF16949 bokan. Servicearin Sabis ɗin Gyare Hadawa zuba jari,yashi,Kushin nauyi, Stauren ɓoye ɓoye,Siffar Centrifugal,Cast Vacuum,Dindindin Mould Gyare, .Hanyoyin iyawa sun hada da EDI, taimakon injiniya, ingantaccen samfuri da aiki na sakandare.
Fitar Masana'antu Abubuwan Nazarin sassa don: Motoci, Bikes, Jirgin sama, kayan kiɗa, Jirgin ruwa, Na'urorin hangen nesa, na'urori masu auna sigina, na'urori masu auna sigina, Na'urori, Kayan lantarki, ,unshi, Clocks, Inji, Injiniya, Kayan Kaya, Kayan Jiki, Jigs, Telecom, Haske, Kayan aikin likita, Na'urar daukar hoto, Robobi, Sassaka, kayan sauti, kayan wasanni, Kayan aiki, Kayan wasa da ƙari.
Me Zamu taimake ku yi gaba?
Je zuwa Shafin Farko Don Mutu Wasa China
→Sassan Kasuwanci-Gano abin da muka aikata.
→ Tallan kwankwasiyya Game da Ayyukan Gyare Mutuwa
By Minghe Mutu Wasa Wasa | Categories: Labarai masu Taimakawa |Material Tags: Gyare Aluminum, Zinc Gyare, Fitar Magnesium, Castan Wasanni, Bakin Karfe Cast, Fitar tagulla,Gyare Tagulla,Fitar Bidiyo,Tarihin Kamfanin,Aluminum Mutu Gyare | Comments Off