Matsayin Mutu-Fitar Hot Mold Machine A Tsarin Zafin Zafin Mutuwa
The mutu-simintin zafi mold inji kuma ake kira mutu-simintin mold zazzabi mai kula. Ikon atomatik na mutu-simintin hot mold machine's mold zafin jiki shine hanyar da ba makawa a cikin fasahar mutuƙar simintin zamani. Mene ne ayyuka na injin mutu-simintin injin ƙonawa a cikin sarrafa zafin jiki na ƙirar mutuƙar?
A cikin Matakin preheating na Mutuwar Gyaran Mutuwar, Matsayin Injin Inji Mai Zafi
- Preheating da mold iya rage yawan molds, inganta samar yadda ya dace da kuma rage sharar gida;
- Preheating da mold iya rage thermal tasiri na gami karfe ruwa a kan mutu-simintin mold, tsawaita lokaci na thermal gajiya fasa a cikin mold, da kuma mika sabis na mold.
- Preheating da masana'antu na iya sa rabe na ɓangaren zamiya na ƙirar ya faɗaɗa da daidaitawa, kuma ya hana karfen ƙarfe ya yi hakowa cikin ɓangaren zamiya kuma ya murƙushe sifar;
Na'urar mutuƙar simintin zafi mai ƙyalƙyali mai ƙyalƙyali ƙyallen za ta iya rage madaidaicin yanayin zafi da rage girgizawar baƙin ƙarfe. An sau da yawa amfani a cikin nauyi karfe simintin mold. The mutu Fitar injin ingin mai zafi yana daɗa ƙyalli daidai gwargwado kuma yana da aikin sanyaya ƙirar don tabbatar da tsayayyen ƙirar ƙirar da rage girman girgizawar ƙarfe mai narkewa; shi ne daidaitattun kayan aiki don samar da aluminium gami-bakin-bango sassa da magnesium alloy casting mold.
Aikin Mutuwar Fitar da Injin Zazzabi Mai zafi a Matakin Sarrafa Zazzabi na Mutuwar
Idan zazzabi mai ƙyalƙyali ya yi yawa ko ya yi ƙasa sosai, zai haifar da rashi kamar girman simintin simintin gyare -gyare, ƙimar ƙin ƙima da rage fitarwa. Lokacin zubar da simintin katanga mai kauri, zafin da ake aikawa zuwa ƙirar sau da yawa ƙasa da zafin da ƙirar ta ɓace, don haka ba za a iya isa ga yanayin zafin da ya dace ba, kuma ana buƙatar injin mutuƙar siminti don ci gaba da ƙara zafi don kiyayewa da mold zazzabi m.
Dangane da yanayin zafin jiki, tasirin ingancin simintin mutuƙar yana da abubuwa masu zuwa.
Ƙananan zafin jiki na mold zai iya haifar da:
- (1) Babban matsin lamba ya yi yawa, kuma simintin gyare -gyaren yana da wahalar faɗi;
- (2) Aikin demoulding na wakilin sakin ƙirar (wanda aka fi sani da kayan sakin ƙirar) yana tabarbarewa;
- (3) Akwai makullan sanyi a saman simintin;
- (4) Bambancin zafin jiki tsakanin ƙirar da ƙarfe mai ruwa ya yi yawa, wanda ke hanzarta lalacewar ƙirar;
- (5) Akwai alamu ko alamomi a saman ƙirar;
- (6) Rashin aiki
Yawan zafin jiki na mold zai iya haifar da:
- (1) Mould mai danko da nakasa;
- (2) Ƙara yawan amfani da wakilin saki da hanzarta bazuwar;
- (3) Rage ƙarar don ƙarawa;
- (4) Sashe mai motsi na ƙirar yana da saurin lalacewa da hanzarin lalacewa;
- (5) Akwai kumfa a saman;
- (6) Akwai ramuka masu raguwa a ciki.
Mutuwar simintin injin injin zafi gabaɗaya yana amfani da mai a matsayin matsakaici, kuma zafin aiki na iya kaiwa 320 ° C. Amma akwai keɓewa, kamar sanyaya murɗaɗɗen ruwa da wasu murjani na ɗakin zafi mai mutuƙar mutuƙar injin injin. Don hana wuta, ana iya amfani da ruwa mai matsa lamba a matsayin matsakaici don hana turɓaya a 140 ° C. Za'a iya amfani da tsarin sanyaya ruwa wanda ba a matsa ba kawai a ƙarƙashin 95 ℃.
A cikin tsarin simintin mutuƙar, zazzabi mai ɗorewa, lokacin cikawa, matsi da zazzabi mai ƙura. Waɗannan sigogi suna da alaƙa da alaƙa da ingancin simintin mutuƙar, fitarwa da rayuwar mold. A cikin samar da mutuƙar simintin, injin ƙyalƙyali mai ƙyalƙyali yana haɓaka inganci da fasaha na sassan mutu-mutu ta hanyar daidaita yanayin zafin jiki, kuma aikinsa da tasirinsa bayyananne ne.
Da fatan za a adana tushe da adireshin wannan labarin don sake bugawa: Matsayin Mutu-Fitar Hot Mold Machine A Tsarin Zafin Zafin Mutuwa
Minghe Kamfanin 'Yan Wasa Masu Mutu aka sadaukar domin tsirar da samar da inganci da kuma high yi Gyare sassa (karfe mutu simintin sassa Range yafi hada da Thin-Wall Mutu Wasa,Hot Chamber Mutu Wasa,Cold Chamber Mutu Wasa), Zagaye Sabis (Mutuwar 'Yan Wasa,CNC machining,Motsa Motsa, Jiyya na sama) .Adadin al'ada Aluminium ya mutu, magnesium ko Zamak / zinc mutu simintin gyare-gyare da sauran buƙatun simintin maraba don tuntube mu.
Karkashin kulawar ISO9001 da TS 16949, Ana aiwatar da dukkan matakai ta hanyar daruruwan injunan jefa simintin da suka mutu, injunan axis 5, da sauran kayan aiki, tun daga masu fashewa zuwa na’urar Ultra Sonic masu wanki.Minghe ba kawai tana da kayan aiki na zamani ba amma kuma tana da kwararru ƙungiyar ƙwararrun injiniyoyi, masu aiki da sufetoci don tabbatar da ƙirar abokin ciniki ta zama gaskiya.
Manufactureran kwangilar masana'antar mutu. Abubuwan haɓakawa sun haɗa da sassan sanyi na sassan mutuɗar aluminum daga 0.15 lbs. zuwa 6 lbs., saurin canje-canje da aka saita, da aikin inji. Sabis-ƙarin ayyuka sun haɗa da gogewa, faɗakarwa, lalatawa, fashewar harbi, zane, zane, rufi, haɗuwa, da kayan aiki. Abubuwan da aka yi aiki tare sun haɗa da allo irin su 360, 380, 383, da 413.
Zinc ya mutu don jefa ƙirar ƙira / sabis na injiniya tare. Custom manufacturer na daidaici tutiya mutu simintin gyaran kafa. Castananan 'yan simintin gyare-gyare, pressurean ƙwanƙwasa masu juzu'in juzu'in simintin gyare-gyaren juzu'ai, ƙera simintin gyare-gyare na al'ada, ɓangaren mutu da' yan wasa masu mutuwa masu zaman kansu da ƙofar da aka hatimce za a iya ƙera su. Za'a iya kerarrar 'yan simintin a tsayi da faɗi har zuwa 24 a ciki. A cikin +/- 0.0005 a cikin. Haƙuri.
ISO 9001: 2015 bokan masana'anta ta mutu magnesium, Abubuwan haɓaka sun haɗa da matsin lamba na magnesium mai matsi mai yawa har zuwa tan 200 mai ɗumi mai zafi & 3000 ton mai sanyi, ƙirar kayan aiki, gogewa, gyare-gyaren, inji, foda & zanen ruwa, cikakken QA tare da damar CMM , taro, marufi & isarwa.
ITAF16949 bokan. Servicearin Sabis ɗin Gyare Hadawa zuba jari,yashi,Kushin nauyi, Stauren ɓoye ɓoye,Siffar Centrifugal,Cast Vacuum,Dindindin Mould Gyare, .Hanyoyin iyawa sun hada da EDI, taimakon injiniya, ingantaccen samfuri da aiki na sakandare.
Fitar Masana'antu Abubuwan Nazarin sassa don: Motoci, Bikes, Jirgin sama, kayan kiɗa, Jirgin ruwa, Na'urorin hangen nesa, na'urori masu auna sigina, na'urori masu auna sigina, Na'urori, Kayan lantarki, ,unshi, Clocks, Inji, Injiniya, Kayan Kaya, Kayan Jiki, Jigs, Telecom, Haske, Kayan aikin likita, Na'urar daukar hoto, Robobi, Sassaka, kayan sauti, kayan wasanni, Kayan aiki, Kayan wasa da ƙari.
Me Zamu taimake ku yi gaba?
Je zuwa Shafin Farko Don Mutu Wasa China
→Sassan Kasuwanci-Gano abin da muka aikata.
→ Tallan kwankwasiyya Game da Ayyukan Gyare Mutuwa
By Minghe Mutu Wasa Wasa | Categories: Labarai masu Taimakawa |Material Tags: Gyare Aluminum, Zinc Gyare, Fitar Magnesium, Castan Wasanni, Bakin Karfe Cast, Fitar tagulla,Gyare Tagulla,Fitar Bidiyo,Tarihin Kamfanin,Aluminum Mutu Gyare | Comments Off