Oxygen-Nitrogen-Carbon Shigar Aluminum Die
Ana iya aiwatar da iskar Oxygen da nitrocarburizing a cikin tanderun carburizing rami, ta amfani da ammoniya mai ruwa, iskar oxygen da nitrogen a matsayin wakilai masu kutse. Bangon ciki na tukunyar tanderu, farfajiyar murfin murhu da firam ɗin da aka ɗora duk an rufe shi da fentin gilashin ruwa kuma ya bushe a 200 ° C don tsawaita rayuwar sabis.
Zazzabi na tanderun da ba komai a cikin tanderun an ɗaga shi zuwa 620 ° C, ana ɗora ƙirar ƙarfe 3Cr2W8V a cikin tanderun, ana shigar da nitrogen a cikin tanderun don cire iska, ƙarancin nitrogen shine 0.4-0.5M / h, kuma matsa lamba shine 20. ×10∧4Pa (2kgf/cm2) Banda iska don 1h. Sa'an nan kuma tada zafin wutar tanderu zuwa 570 ℃, dakatar da kwararar nitrogen, kuma canza kwararar iskar gas ammonia tare da nauyin 0.5-0.6m3 da matsa lamba na 7 × 10∧4Pa (7kgf/cm2). A lokaci guda, iskar oxygen tare da ƙimar 50-80mL / min da matsa lamba Yana da 3 × 10∧ 4Pa (0.3kgf / cm2).
Bayan an ajiye shi a 570 ° C na 2h, ana tayar da zafin wutar tanderu zuwa 620 ° C kuma a ajiye shi don 2h, kuma tsarin kulawa ya ƙare. Yanke ammonia da oxygen, canza zuwa nitrogen don shayar da ammonia da oxygen a cikin tanderun, kuma yanke wutar lantarki don rage zafin wutar tanderu. Lokacin da tanderun zafin jiki ya faɗi ƙasa da 450 ℃, cire mold daga cikin tanderun kuma saka shi a cikin bangon tanki Sannu a hankali kwantar da zafin jiki a cikin tanki mai sanyaya da ruwa.
Bayan co-infiltration, da surface taurin ne 891HV0.05, da surface Layer ne fari da haske epsilon Layer, kauri ne 0.02-0.023mm, babban nitride matakai ne Fe3N da Fe4N, kuma akwai wani karamin adadin Fe3O4, da kuma babu bayyanannen lokaci na Fe2N. Haɗawa zuwa ε shine N-dauke da α-Fe yaduwa Layer, kuma jimillar nitriding zurfin farin Layer mai haske tare da yaduwa Layer shine 0.2-0.28mm. Zuciya ce tsohuwar nama + jikin kebul mai zafin rai.
Fiye da guda dubu na 3Cr2W8V karfe aluminum alloy mutu-simintin gyare-gyaren da aka yi amfani da su ta hanyar tsarin da ke sama an mutu-siminti, kuma saman har yanzu yana da santsi kuma yana da kyau, kuma rushewar yana da santsi, ba tare da mannewa, bawo, scratches, da lalata.
Da fatan za a adana tushe da adireshin wannan labarin don sake bugawa:Oxygen-Nitrogen-Carbon Shigar Aluminum Die
Minghe Kamfanin 'Yan Wasa Masu Mutu aka sadaukar domin tsirar da samar da inganci da kuma high yi Gyare sassa (karfe mutu simintin sassa Range yafi hada da Thin-Wall Mutu Wasa,Hot Chamber Mutu Wasa,Cold Chamber Mutu Wasa), Zagaye Sabis (Mutuwar 'Yan Wasa,CNC machining,Motsa Motsa, Jiyya na sama) .Adadin al'ada Aluminium ya mutu, magnesium ko Zamak / zinc mutu simintin gyare-gyare da sauran buƙatun simintin maraba don tuntube mu.
Karkashin kulawar ISO9001 da TS 16949, Ana aiwatar da dukkan matakai ta hanyar daruruwan injunan jefa simintin da suka mutu, injunan axis 5, da sauran kayan aiki, tun daga masu fashewa zuwa na’urar Ultra Sonic masu wanki.Minghe ba kawai tana da kayan aiki na zamani ba amma kuma tana da kwararru ƙungiyar ƙwararrun injiniyoyi, masu aiki da sufetoci don tabbatar da ƙirar abokin ciniki ta zama gaskiya.
Manufactureran kwangilar masana'antar mutu. Abubuwan haɓakawa sun haɗa da sassan sanyi na sassan mutuɗar aluminum daga 0.15 lbs. zuwa 6 lbs., saurin canje-canje da aka saita, da aikin inji. Sabis-ƙarin ayyuka sun haɗa da gogewa, faɗakarwa, lalatawa, fashewar harbi, zane, zane, rufi, haɗuwa, da kayan aiki. Abubuwan da aka yi aiki tare sun haɗa da allo irin su 360, 380, 383, da 413.
Zinc ya mutu don jefa ƙirar ƙira / sabis na injiniya tare. Custom manufacturer na daidaici tutiya mutu simintin gyaran kafa. Castananan 'yan simintin gyare-gyare, pressurean ƙwanƙwasa masu juzu'in juzu'in simintin gyare-gyaren juzu'ai, ƙera simintin gyare-gyare na al'ada, ɓangaren mutu da' yan wasa masu mutuwa masu zaman kansu da ƙofar da aka hatimce za a iya ƙera su. Za'a iya kerarrar 'yan simintin a tsayi da faɗi har zuwa 24 a ciki. A cikin +/- 0.0005 a cikin. Haƙuri.
ISO 9001: 2015 bokan masana'anta ta mutu magnesium, Abubuwan haɓaka sun haɗa da matsin lamba na magnesium mai matsi mai yawa har zuwa tan 200 mai ɗumi mai zafi & 3000 ton mai sanyi, ƙirar kayan aiki, gogewa, gyare-gyaren, inji, foda & zanen ruwa, cikakken QA tare da damar CMM , taro, marufi & isarwa.
ITAF16949 bokan. Servicearin Sabis ɗin Gyare Hadawa zuba jari,yashi,Kushin nauyi, Stauren ɓoye ɓoye,Siffar Centrifugal,Cast Vacuum,Dindindin Mould Gyare, .Hanyoyin iyawa sun hada da EDI, taimakon injiniya, ingantaccen samfuri da aiki na sakandare.
Fitar Masana'antu Abubuwan Nazarin sassa don: Motoci, Bikes, Jirgin sama, kayan kiɗa, Jirgin ruwa, Na'urorin hangen nesa, na'urori masu auna sigina, na'urori masu auna sigina, Na'urori, Kayan lantarki, ,unshi, Clocks, Inji, Injiniya, Kayan Kaya, Kayan Jiki, Jigs, Telecom, Haske, Kayan aikin likita, Na'urar daukar hoto, Robobi, Sassaka, kayan sauti, kayan wasanni, Kayan aiki, Kayan wasa da ƙari.
Me Zamu taimake ku yi gaba?
Je zuwa Shafin Farko Don Mutu Wasa China
→Sassan Kasuwanci-Gano abin da muka aikata.
→ Tallan kwankwasiyya Game da Ayyukan Gyare Mutuwa
By Minghe Mutu Wasa Wasa | Categories: Labarai masu Taimakawa |Material Tags: Gyare Aluminum, Zinc Gyare, Fitar Magnesium, Castan Wasanni, Bakin Karfe Cast, Fitar tagulla,Gyare Tagulla,Fitar Bidiyo,Tarihin Kamfanin,Aluminum Mutu Gyare | Comments Off