Ƙirƙira shi ne sunan gama -gari na ƙirƙira da tambura. Hanya ce ta kerawa da sarrafawa wacce ke amfani da guduma, anvil, na’urar injin ƙirƙira ko mutu don amfani da matsin lamba a cikin komai don samar da gurɓataccen filastik, don samun sifa da girman aikin da ake buƙata. .
A cikin tsarin ƙirƙirawa, gabaɗayan billet ɗin yana fama da nakasa na filastik kuma yana da yawan adadin kwararar filastik; a cikin tsarin buga tambarin, an ƙirƙira takardar ta musamman ta hanyar canza matsayin sararin kowane yanki, kuma babu babban kwararar filastik mai gudana a ciki. Ƙirƙiri galibi ana amfani da shi don sarrafa sassan ƙarfe, kuma ana iya amfani da shi don sarrafa wasu abubuwan da ba ƙarfe ba, kamar robobi na injiniya, roba, ɓoyayyiyar yumɓu, ɓoyayyun bulo, da kuma samar da kayan haɗin gwiwa.
Yin ƙirƙira da mirginawa da zane a cikin masana'antar ƙarfe duk aikin filastik ne, ko sarrafa matsa lamba, amma galibi ana amfani da ƙirƙira don samar da sassan ƙarfe, yayin da mirgina da zane galibi ana amfani da su don samar da faranti, tube, bututu, da sauransu Janar. -inyi niyyar kayan ƙarfe kamar bayanan martaba da wayoyi.
A ƙarshen zamanin Neolithic, mutane sun fara haƙa jan jan ƙarfe na halitta don yin kayan ado da ƙananan abubuwa. Kasar Sin ta yi amfani da tsarin kirkirar sanyi don yin kayan aiki a kusan 2000 BC. Misali, jajayen kayan jan ƙarfe da aka tono daga rukunin al'adun Qijia na Huangniangtai a Wuwei, Gansu suna da alamun hammata. A tsakiyar Daular Shang, an yi amfani da baƙin ƙarfe na meteorite don kera makamai, ta amfani da tsarin ƙirƙira dumama. Ginin ƙarfe mai ƙamshi wanda ya bayyana a ƙarshen lokacin bazara da lokacin kaka an ƙirƙira shi ta hanyar maimaita dumama da ƙirƙira don fitar da abubuwan hada oxide.
Da farko, mutane *sun nannade guduma don ƙirƙira, daga baya kuma wata hanyar ɗaga babban guduma ta hanyar jan igiya da kura sannan kuma ta faɗi da yardar kaina don ƙirƙirar ɓoyayyun ɓoyayyu. Bayan karni na 14, ƙarfin dabbar da jujjuyawar hydraulic ya bayyana.
A cikin 1842, Nasmith na Burtaniya ya yi hamma na tururi na farko, yana kawo ƙirƙira cikin zamanin ikon amfani. Daga baya, ƙirƙiro madatsar ruwa ta ruwa, guduma mai goge-goge mai motsi, ƙera gudumawar iska da injinan inji sun bayyana ɗaya bayan ɗaya. An fara amfani da gudumawar goge-goge a lokacin Yaƙin Basasa na Amurka (1861-1865) don mutuƙar ƙera sassan makami, sannan turmutsitsin ƙirƙira guduma ya bayyana a Turai, kuma sannu a hankali an inganta fasahar mutuƙar ƙirƙira. Ya zuwa ƙarshen karni na 19, an ƙirƙiri babban nau'in kayan aikin ƙirƙira na zamani.
A farkon karni na 20, tare da fara samar da motoci da yawa, ƙirar mutuƙar zafi ta haɓaka cikin sauri kuma ta zama babban tsarin ƙirƙirawa. A tsakiyar karni na 20, injin mutuƙar ƙirƙira mai zafi, injin ƙirar lebur da guduma mara ƙamshi a hankali ya maye gurbin hammata na yau da kullun, haɓaka yawan aiki da rage rawar jiki da hayaniya. Tare da haɓaka sabbin matakai na ƙirƙira abubuwa kamar ƙirƙira blanks tare da ƙarancin fasaha ba tare da ƙonawa ba, madaidaiciyar madaidaiciya da ƙirar rayuwa mai tsawo, zafi mai zafi, ƙirƙirar juyawa, da ƙirƙira magudi, magudi, da layukan samarwa na atomatik, inganci da tattalin arziƙi illolin samar da jabu na ci gaba da inganta.
Bayyanar jabu na sanyi yana gab da ƙirƙira zafi. Farkon jan ƙarfe, zinariya, flakes na azurfa da tsabar kuɗi duk jabu ne na jabu. An yi amfani da aikace -aikacen ƙirƙira sanyi a masana'antar kera a cikin karni na 20. Maganar sanyi, fitowar sanyi, ƙirƙira radial, da jujjuyawar juzu'i an haɓaka su a jere, sannu a hankali suna samar da ingantaccen tsarin ƙirƙira wanda zai iya samar da sassan daidai ba tare da yankewa ba.
Tambarin farko kawai yayi amfani da kayan aiki masu sauƙi kamar shebur, sausaya, huɗu, gudumawar hannu, da alfasha don ƙirƙirar zanen ƙarfe (galibi faranti na jan ƙarfe ko jan ƙarfe, da dai sauransu) ta hanyar yankan hannu, bugun hannu, shebur, da raɗaɗi. Ƙera gongs, kuge da sauran kayan kida da tukwane. Tare da ƙaruwa a cikin fitarwa na faranti na matsakaici da kauri da haɓaka haɓakar matatun mai na hydraulic da injinan injinan, aikin hatimin shima ya fara aiki a tsakiyar ƙarni na 19.
A cikin 1905, Amurka ta fara kera baƙin ƙarfe mai ɗorewa mai ɗorewa a cikin coils. A shekara ta 1926, ta fara kera baƙin ƙarfe mai faɗi. Daga baya, ƙarfe mai ci gaba da birgima. A lokaci guda, ana ƙara fitar da faranti da tube, ana inganta inganci, kuma ana rage farashi. Haɗe tare da haɓaka keɓaɓɓun jiragen ruwa, motocin jirgin ƙasa, tukunyar jirgi, kwantena, motoci, gwangwani, da sauransu, stamping ya zama ɗaya daga cikin hanyoyin da aka fi amfani da su.
Ƙirƙirawa galibi ana rarrabasu gwargwadon hanyar da aka kafa da zafin zafin. Dangane da hanyar kafawa, ana iya raba ƙirƙira zuwa ƙirƙira da hatimi; gwargwadon yanayin naƙasasshe, za a iya raba ƙirƙira zuwa ƙirƙira mai zafi, ƙirƙira mai sanyi, ƙirƙira mai ɗumi da ƙirƙira isothermal.
Ana yin ƙirƙira mai zafi sama da zafin sake sake ƙirƙira ƙarfe. Ƙara yawan zafin jiki zai iya inganta ƙwayar filastik na karfe, wanda ke da amfani don inganta yanayin ciki na aikin aiki kuma yana da wuya a fashe. Babban zafin jiki kuma na iya rage juriyar gurɓacewar ƙarfe da rage yawan injin ƙirƙira da ake buƙata. Duk da haka, akwai da yawa zafi ƙirƙira tafiyar matakai, daidaitattun workpiece ne matalauta, da surface ba santsi, da kuma ƙirƙira ne yiwuwa ga hadawan abu da iskar shaka, decarburization da kona.
Ƙirƙira mai sanyi abu ne na jabu da ake yi a zafin jiki mafi ƙanƙanta da zafin zafin recrystallization na ƙarfe. Gabaɗaya magana, ƙirƙira mai sanyi yana nufin musamman don ƙirƙirawa a cikin zafin jiki na ɗaki, kuma ƙirƙirawa a zafin jiki sama da zafin ɗaki amma ba ya wuce zafin zafin sake maimaitawa ana kiransa zafin jiki. Ƙirƙira. Ƙirƙira mai ɗumi yana da madaidaicin madaidaici, shimfida mai laushi da ƙarancin juriya.
Kayan aikin da aka ƙirƙira ta hanyar ƙirƙira sanyi a ɗakin zafin jiki yana da babban siffa da daidaiton girman, shimfida mai santsi, ƙarancin hanyoyin sarrafawa, da sauƙin sarrafawa ta atomatik. Za'a iya amfani da yawancin abubuwan da ake ƙirƙirawa da sanyi da sassan tambarin sanyi azaman sassa ko samfura ba tare da yanke sarrafawa ba. Koyaya, a lokacin ƙirƙirawar sanyi, saboda ƙarancin filastik na ƙarfe, yana da sauƙin fashewa yayin ɓarna, kuma rashin juriya yana da girma, yana buƙatar manyan injunan tonar ƙarfe.
Ƙirƙirar isothermal yana nufin cewa zazzabi na sarari ya kasance mai ɗorewa a duk lokacin aiwatar da tsari. Ƙirƙirar isothermal shine yin cikakken amfani da babban filastik na wasu karafa a yanayin zafi, ko don samun takamaiman tsari da kaddarori. Ƙirƙirar isothermal yana buƙatar mutu da blank a ajiye su a cikin zafin jiki na dindindin, wanda ke buƙatar tsada mai tsada kuma ana amfani da shi ne kawai don ayyukan ƙirƙira na musamman, kamar ƙirar superplastic.
Yin ƙirƙira na iya canza tsarin ƙarfe da haɓaka kaddarorin ƙarfe. Bayan da ingot yayi zafi na jabu, ainihin as-cast looseness, pores, microcracks, da dai sauransu ana matsawa ko waldi; ainihin dendritic lu'ulu'u sun karye don sa hatsi su yi kyau; a lokaci guda, ana canza rarrabuwa ta asali da rashin daidaituwa Rarraba don sa ƙungiyar ta zama ɗaya, ta yadda za a sami gafara tare da ƙaƙƙarfan ciki, daidaituwa, fineness, kyakkyawan aiki gaba ɗaya, da amintaccen amfani. Bayan ƙirƙira naƙasasshe ta hanyar ƙirƙira mai zafi, ƙarfe tsarin fibrous ne; bayan ƙirƙirawar ta lalace, lu'ulu'u na ƙarfe suna cikin tsari.
Ƙirƙirawa shine kwararar filastik na ƙarfe don yin kayan aikin da ake so. Ofarar ƙarfe ba ta canzawa bayan haɓakar filastik ta hanyar ƙarfin waje, kuma ƙarfen koyaushe yana gudana zuwa ɓangaren tare da mafi ƙarancin juriya. A cikin samarwa, ana sarrafa fasalin abin aiki daidai da waɗannan ƙa'idodin don a samu nakasu kamar ɓacin rai da zane, sakewa, lankwasawa, da zane.
Girman kayan aikin da aka ƙirƙira daidai ne, wanda ya dace da ƙungiyar samar da taro. The girma na mutu ƙirƙira, extrusion, stamping da sauran aikace -aikace ne daidai da barga. Za'a iya amfani da ingantaccen ƙirar ƙera kayan masarufi da layin samar da ƙirƙira ta atomatik don tsara taro na musamman ko samarwa da yawa.
Tsarin samarwa na ƙirƙira ya haɗa da faffadar fa'ida kafin yin tsari, dumama da kuma yin rigakafin blanks; jiyya mai zafi, tsaftacewa, daidaitawa da duba kayan aiki bayan kafa. Injunan da ake amfani da su na jabu sun hada da yin jabun guduma, injinan hydraulic da injinan inji. Hammer mai ƙirƙira yana da babban tasirin tasiri, wanda ke dacewa da kwararar filastik na ƙarfe, amma zai haifar da girgiza; injin hydraulic yana amfani da ƙirƙira a tsaye, wanda ya dace don ƙera ƙarfe ta hanyar inganta tsarin, kuma aikin yana da tsayayye, amma yawan aiki ba shi da yawa; injin injin yana da tsayayyen bugun jini kuma yana da sauƙin gane injiniya da sarrafa kansa.
A nan gaba, tsarin ƙirƙira zai inganta ingancin ciki na sassan ƙirƙira, haɓaka madaidaiciyar ƙirƙira da fasaha madaidaiciya, haɓaka kayan aikin ƙirƙira da ƙirƙira layukan samarwa tare da haɓaka yawan aiki da aiki da kai, haɓaka sassauƙan ƙirƙira tsarin, haɓaka sabbin kayan ƙirƙira da sarrafa jabu. hanyoyin, da sauransu suna haɓaka.
Inganta ingancin cikin gida na gafartawa shine musamman don haɓaka kaddarorin injinan su (ƙarfi, filastik, tauri, ƙarfin gajiya) da dogaro. Wannan yana buƙatar mafi kyawun aikace -aikacen ka'idar gurɓataccen filastik. aikace -aikacen kayan tare da mafi kyawun inganci; daidai pre-ƙirƙira dumama da ƙirƙira zafi magani; mafi tsauri kuma mafi girman gwajin da ba a lalata ba na sassan jabu.
Kadan kuma babu yankan aiki shine mafi mahimmancin ma'auni da jagora ga masana'antar injin don haɓaka amfani da kayan, haɓaka yawan aiki da rage yawan kuzari. Ƙananan ƙirƙira blanks, babu dumama oxyidation, kazalika da haɓaka babban-taurin kai, mai jurewa, kayan kwalliya na tsawon rai da hanyoyin kula da farfajiya, zai zama mai dacewa ga faɗaɗa aikace-aikacen daidaitaccen ƙirƙira da madaidaicin hatimi.
Da fatan za a adana tushe da adireshin wannan labarin don sake bugawa: Karya maganar fasaha
Minghe Kamfanin 'Yan Wasa Masu Mutu aka sadaukar domin tsirar da samar da inganci da kuma high yi Gyare sassa (karfe mutu simintin sassa Range yafi hada da Thin-Wall Mutu Wasa,Hot Chamber Mutu Wasa,Cold Chamber Mutu Wasa), Zagaye Sabis (Mutuwar 'Yan Wasa,CNC machining,Motsa Motsa, Jiyya na sama) .Adadin al'ada Aluminium ya mutu, magnesium ko Zamak / zinc mutu simintin gyare-gyare da sauran buƙatun simintin maraba don tuntube mu.
Karkashin kulawar ISO9001 da TS 16949, Ana aiwatar da dukkan matakai ta hanyar daruruwan injunan jefa simintin da suka mutu, injunan axis 5, da sauran kayan aiki, tun daga masu fashewa zuwa na’urar Ultra Sonic masu wanki.Minghe ba kawai tana da kayan aiki na zamani ba amma kuma tana da kwararru ƙungiyar ƙwararrun injiniyoyi, masu aiki da sufetoci don tabbatar da ƙirar abokin ciniki ta zama gaskiya.
Manufactureran kwangilar masana'antar mutu. Abubuwan haɓakawa sun haɗa da sassan sanyi na sassan mutuɗar aluminum daga 0.15 lbs. zuwa 6 lbs., saurin canje-canje da aka saita, da aikin inji. Sabis-ƙarin ayyuka sun haɗa da gogewa, faɗakarwa, lalatawa, fashewar harbi, zane, zane, rufi, haɗuwa, da kayan aiki. Abubuwan da aka yi aiki tare sun haɗa da allo irin su 360, 380, 383, da 413.
Zinc ya mutu don jefa ƙirar ƙira / sabis na injiniya tare. Custom manufacturer na daidaici tutiya mutu simintin gyaran kafa. Castananan 'yan simintin gyare-gyare, pressurean ƙwanƙwasa masu juzu'in juzu'in simintin gyare-gyaren juzu'ai, ƙera simintin gyare-gyare na al'ada, ɓangaren mutu da' yan wasa masu mutuwa masu zaman kansu da ƙofar da aka hatimce za a iya ƙera su. Za'a iya kerarrar 'yan simintin a tsayi da faɗi har zuwa 24 a ciki. A cikin +/- 0.0005 a cikin. Haƙuri.
ISO 9001: 2015 bokan masana'anta ta mutu magnesium, Abubuwan haɓaka sun haɗa da matsin lamba na magnesium mai matsi mai yawa har zuwa tan 200 mai ɗumi mai zafi & 3000 ton mai sanyi, ƙirar kayan aiki, gogewa, gyare-gyaren, inji, foda & zanen ruwa, cikakken QA tare da damar CMM , taro, marufi & isarwa.
ITAF16949 bokan. Servicearin Sabis ɗin Gyare Hadawa zuba jari,yashi,Kushin nauyi, Stauren ɓoye ɓoye,Siffar Centrifugal,Cast Vacuum,Dindindin Mould Gyare, .Hanyoyin iyawa sun hada da EDI, taimakon injiniya, ingantaccen samfuri da aiki na sakandare.
Fitar Masana'antu Abubuwan Nazarin sassa don: Motoci, Bikes, Jirgin sama, kayan kiɗa, Jirgin ruwa, Na'urorin hangen nesa, na'urori masu auna sigina, na'urori masu auna sigina, Na'urori, Kayan lantarki, ,unshi, Clocks, Inji, Injiniya, Kayan Kaya, Kayan Jiki, Jigs, Telecom, Haske, Kayan aikin likita, Na'urar daukar hoto, Robobi, Sassaka, kayan sauti, kayan wasanni, Kayan aiki, Kayan wasa da ƙari.
Me Zamu taimake ku yi gaba?
Je zuwa Shafin Farko Don Mutu Wasa China
→Sassan Kasuwanci-Gano abin da muka aikata.
→ Tallan kwankwasiyya Game da Ayyukan Gyare Mutuwa
By Minghe Mutu Wasa Wasa | Categories: Labarai masu Taimakawa |Material Tags: Gyare Aluminum, Zinc Gyare, Fitar Magnesium, Castan Wasanni, Bakin Karfe Cast, Fitar tagulla,Gyare Tagulla,Fitar Bidiyo,Tarihin Kamfanin,Aluminum Mutu Gyare | Comments Off